FSB fluoride plastic chemical pump in the daily use of the process, the failure encountered, it is impossible to do, then you know FSB Fluoroplastic Chemical Pump What are the common failures? And what should be done to exclude? Then introduce you to FSB Fluoroplastic Chemical Pump common failure and troubleshooting. FSB fluorine plastic chemical pump common failure and troubleshooting methods First, FSB fluorine plastic chemical pump can not play the liquid (a) reasons 1, the suction tube air, the entrance obstruction; 2, the suction height is too high; 3, Head; 4, exhaust pipe is too thin. Pipeline loss is too large; 5, reverse. (B) the exclusion method 1, clean up the pipeline, the net discharge of air; 2, reducing the installation height of the pump; 3, more head large pump; 4, caliber and pump outlet and other large output; Second, the lack of flow of FSB fluorine plastic chemical pump (a) the reasons 1, the impeller damage; 2, seal damage; 3, the number of deficiencies; 4, the inlet pipe is too small; 5, excessive outlet pipe elbow, resistance is too large. (B) the exclusion method 1, update the impeller; 2, seals; 3, increase the number of revolutions; 4, according to the provisions of pipelines; Third, the FSB fluorine plastic chemical pump head inadequate (a) reasons 1, the transmission medium containing gas or medium viscosity is too large; 2, impeller and blade damage; 3, the number of revolutions is not enough. (B) the exclusion method 1, reduce the viscosity of the medium or increase injection pressure; 2, replace the impeller; 3, increase the number of revolutions. Four, FSB fluorine plastic chemical pump shaft end leakage (a) reasons 1, the mechanical seal snap ring too loose; 2, the shaft end snap ring transition size gap is too large. (B) the exclusion method 1, tighten the card bad two hexagonal screw ruthenium; 2, the pump removal, the shaft, the card stuck around the F4 raw material with a few laps film. Five, FSB fluorine plastic chemical pump seal leak serious (a) reasons 1, seal material selection improper; 2, grinding 瘵 pay serious wear and tear; 3, moving ring kiss is not; (B) the exclusion method 1, to the pump string describes the situation of the media, with appropriate moving ring; 2, and more wear pieces and adjust the spring pressure to reduce wear and tear; 3, Position; 4, the entire pump disassembly. Swing ring installed on demand seal assembly and the shaft vertical error VI, FSB fluorine plastic chemical pump pump noise or pump vibration (a) reasons 1, the shaft and the motor shaft is not the same heart ; 2, the flow exceeds the use of cavitation; 3, pump cavitation; 4, motor and bearing wear. (B) the exclusion method 1, the correction of pump shaft center; 2, the selection of the appropriate pump. Press the pump to use the scope of operation; 3, reducing the temperature of the medium or increase perfusion pressure; 4, cleaning or bearings. Extended reading: China Construction Water Exhibition water pump manufacturers rankings ptc exhibition motor top ten brands pump valve pipe fittings Show Information Industry Internet (Xiamen) Technology Co., Ltd. Asia Pump Network Editor: He Duanhui (QQ / WeChat:) http: // mj .liuti.cn / (Service Hotline:)

We can do scroll cut service according to design of the client. Scroll cuting can well save materials during production.

1. Technical standard: BS EN 10202, DIN EN 10203, GB/T2520 , JIS G3303

2. Steel type: MR, SPCC
3. Thickness: 0.115 - 0.50 mm
4. Width:  600 - 1050 mm
5. Length: 600-1200mm
Tin Coating: ordinary 2.8 or 2.8g and 5.6g or 5.6g, we can produce according to customer's requests

Scroll Cut Tinplate Sheet

Scroll Cut Tinplate Sheet,Mini Slitting Machine,Tin Mill Black Plate,Tanged Tinplate

Jiangsu Guolian New Material Co., Ltd. , https://www.cntinplate.com